Main Entry - Personal NameGolecruz, R.B.
 Mena, Ph.D. M.G.
Title StatementThe reduction behavior of nickel in high-iron laterites under co/co2/N2 atmospheres
by R.B. Golecruz, M.G
Physical Description63-70 illustrations,graphs
Summary, Etc.The reduction behavior of nickel in high-iron Nonoc laterite was studied by varying the reduction temperature, reaction time and gas composition. It was observed that over a wide range of conditions, the degree of metallization increases with increasing level of any process variable, reaches some peak values, and then decreases with further increase in severity of reduction conditions. It was also noted that no more than 96.6% nickel can be metallized from the test sample. Ammoniacal leaching of pre-reduced pellets demonstrated that the Nonoc laterite is responsive to the treatment. An overall nickel recovery of about 94% is possible with this process
 
     
 
Physical Location
 
     
 
Digital Copy
Not Available
 
     
 
         
         
Online Catalog
Basic Search
Advanced Search
Browse Subjects
Book Cart
 
         

Text Size:
S  -  M  -  L
Copyright © 2004-2025. Philippine eLib Project
Host: U.P. Diliman University Library